Başlık: | Characterisations of CoFeCu films: Influence of Fe concentration |
Yazarlar: | Koçkar, Hakan Özergin, Ercüment Karaağaç, Öznur Uludağ Üniversitesi/Fen-Edebiyat Fakültesi/Fizik Bölümü. Alper, Mürsel AAG-8795-2021 7005719283 |
Anahtar kelimeler: | CoFeCu films Electrodeposition Microstructure Magnetic properties Nife alloy-films Co-Cu films Magnetic-properties Iron films Electrodeposited cobalt Cathode potentials Rotating substrate Electrolyte ph Wave-forms Thin-films Chemistry Materials science Metallurgy & metallurgical engineering Coercive force Crystal structure Electrolytes Magnetoresistance Saturation magnetization X ray diffraction Anisotropic magnetoresistance Body-centered cubic Compositional analysis Face-centered cubic Hexagonal close packed Surface morphology analysis Transverse magnetoresistance Vibrating sample magnetometer Concentration (process) |
Yayın Tarihi: | 15-Şub-2014 |
Yayıncı: | Elsevier |
Atıf: | Koçkar, H. vd. (2014). "Characterisations of CoFeCu films: Influence of Fe concentration". Journal of Alloys and Compounds, 586(Supplement 1), S326-S330. |
Özet: | The properties of electrodeposited CoFeCu films were studied with respect to Fe ion concentration in the electrolyte due to their interesting magnetic properties like high saturation magnetisation and low coercivity. The films were characterised in terms of microstructural and magnetic properties. From the compositional analysis, the Fe contents in the films are found to be consistent with the Fe ion concentrations in the electrolytes. With the surface morphology analysis of the films, the number of the roundish shape structures on the surface increased with increasing Fe ion concentration (>= 0.01 M Fe) whereas the CoCu films (0 M Fe) had ridged grains. The crystal structure of the films, examined by X-ray diffraction, changed from the mixed phase of the hexagonal close packed and face centered cubic (fcc) to the fcc and finally body centered cubic structure as the Fe ion concentration in the electrolyte increased from 0 to 0.04 M. And, the average grain size decreased with increasing Fe ion concentration. Magnetisation measurements by vibrating sample magnetometer displayed that the saturation magnetisation increased and the coercivity decreased as the Fe ion concentration increased. Also, it was found that the easy-axis of the magnetisation of films is parallel to the film plane. All films showed anisotropic magnetoresistance. The longitudinal and transverse magnetoresistance magnitudes of the films changed between 3.2-4.0 and 3.0-3.8, respectively. In the study, considerable differences in the microstructural and magnetic properties were observed and might be ascribed to the change of film content caused by the Fe ion concentration in the electrolyte. A high value of saturation magnetisation, M-s (1797 emu/cm(3)) is achieved under study. |
URI: | https://doi.org/10.1016/j.jallcom.2013.02.167 https://www.sciencedirect.com/science/article/pii/S0925838813005045 http://hdl.handle.net/11452/27239 |
ISSN: | 0925-8388 1873-4669 |
Koleksiyonlarda Görünür: | Scopus Web of Science |
Bu öğenin dosyaları:
Bu öğeyle ilişkili dosya bulunmamaktadır.
DSpace'deki bütün öğeler, aksi belirtilmedikçe, tüm hakları saklı tutulmak şartıyla telif hakkı ile korunmaktadır.